Material Grade | SS430 |
T-430:
This type required custom manufacturing due to basic ferritic non-heat treatable stainless steel which offers good corrosion and oxidation resistance.
Carbon [C] | Manganese [Mn] | Phosphorus [P] | Sulfur [S] | Silicon [Si] | Chromium [Cr] | Nickel [Ni] |
0.12 Max | 1.0 Max | 0.04 Max | 0.03 Max | 1.00 Max | 16.00–18.00 | 0.50 MAX |
Material Grade | SS430 |
T-430:
This type required custom manufacturing due to basic ferritic non-heat treatable stainless steel which offers good corrosion and oxidation resistance.
Carbon [C] | Manganese [Mn] | Phosphorus [P] | Sulfur [S] | Silicon [Si] | Chromium [Cr] | Nickel [Ni] |
0.12 Max | 1.0 Max | 0.04 Max | 0.03 Max | 1.00 Max | 16.00–18.00 | 0.50 MAX |